Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melting Point = 282 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 282 - 293 °C
540 - 559 °F
PolyOne Trilliant™ HC HC6620-0033 RS Natural Polyamide 66 (Nylon 66)
The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead..
Melting Point 282 °C
540 °F
Crystalline, Peak; ASTM D3418
Quadrant EPP Techtron® 1000 PPS Extruded Polyphenylene Sulfide (ASTM Product Data Sheet)
Melting Point 282 °C
540 °F
Crystalline, Peak; ASTM D3418
Quadrant EPP Techtron® PSBG PPS, Polyphenylene sulfide, bearing grade, compression molded (ASTM Product Data Sheet)
Melting Point 282 °C
540 °F
Crystalline, Peak; ASTM D3418
Quadrant EPP Techtron® PSGF PPS - Compression Molded 40% Glass Reinforced Polyphenylene Sulfide (ASTM Product Data Sheet)
Melting Point 282 °C
540 °F
ASTM D3417
Quantum PPS
Information provided by Quantum Advanced Engineering Plastics
Melting Point 282 °C
540 °F
Toyobo TS101 PPS, Glass Fiber/Mineral Reinforced
Key Feature: High dimensional stabilityHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo. Excellent..
Melting Point 282 °C
540 °F
Toyobo TS301 PPS, 30% Glass Fiber Reinforced
Key Feature: Excellent impact resistance, high flowHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo..
Melting Point 282 °C
540 °F
Toyobo TS401 HS PPS, 40% Glass Fiber Reinforced
Key Feature: High toughness, high flow. Features high weld strength.High performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology d..
Melting Point 282 °C
540 °F
Toyobo TS401 PPS, 40% Glass Fiber Reinforced
Key Feature: General Purpose Grade - balanced characteristics suitable for a broad range of uses.High performance injection-molding resin created from crystalline polyphenylene sulfide, using a spec..
Melting Point 282 °C
540 °F
Toyobo TS501 PPS, 50% Glass Fiber Reinforced
Key Feature: High stiffnessHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo. Excellent physical, e..
Melting Point 282 °C
540 °F
Toyobo TS201 HS PPS, Glass Fiber/Mineral Reinforced
Key Feature: High stiffness, high toughnessHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo. Excel..
Melting Point 282 °C
540 °F
Toyobo TS201 PPS, Glass Fiber/Mineral Reinforced
Key Feature: Standard high stiffness - used for metal replacementHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology devel..
Melting Point 282 °C
540 °F
10°C/min; ISO 11357-1/-3
DSM Stanyl® OCD2100 BK27021 PA46-GF40
40% Glass Reinforced, Heat Stabilized
Melting Point 282 °C
540 °F
10°C/min; ISO 11357-1/-3
DSM Stanyl® OCD2300 BLK PA46-GF50
50% Glass Reinforced, Heat Stabilized
Melting Point 282 °C
540 °F
ASTM D2133
Ensinger TECATRON™ GF 40 Polyphenylene sulfide (PPS)
TECATRON PPS is a high performance thermoplastic that combines good mechanical properties with excellent thermal and chemical resistance properties. There is no known solvent that dissolves TECATRON..
Melting Point 282 °C
540 °F
ASTM D2133
Ensinger TECATRON™ PPS Polyphenylene sulfide (PPS)
TECATRON PPS is a high performance thermoplastic that combines good mechanical properties with excellent thermal and chemical resistance properties. There is no known solvent that dissolves TECATRON..
Melting Point 282 °C
540 °F
ASTM D2133
Ensinger TECATRON™ PVX Polyphenylene sulfide (PPS), Bearing Grade
TECATRON PPS is a high performance thermoplastic that combines good mechanical properties with excellent thermal and chemical resistance properties. There is no known solvent that dissolves TECATRON..
Melting Point 282 - 295 °C
540 - 563 °F
Average value: 295 °C Grade Count:81
Overview of materials for Nylon 46, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values ..
Melting Point 282 °C
540 °F
ASTM D2133
Ensinger ENSIFIDE® PPS (Polyphenylene Sulfide) - Extruded Products  (discontinued **)
ENSIFIDE is a high performance thermoplastic that combines good mechanical properties with excellent thermal and chemical resistance properties. There is no known solvent that dissolves ENSIFIDE at..
Copyright © lookpolymers.com All Rights Reserved