Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Quadrant EPP Techtron® PSGF PPS - Compression Molded 40% Glass Reinforced Polyphenylene Sulfide (ASTM Product Data Sheet)

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Manufacturer Quadrant Engineering Plastics Products
Trade Name Techtron®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quadrant EPP Techtron® PSGF PPS - Compression Molded 40% Glass Reinforced Polyphenylene Sulfide (ASTM Product Data Sheet).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.70 g/cc
1.70 g/cc
ASTM D792
Water Absorption 0.020 %
0.020 %
Immersion, 24hr; ASTM D570(2)
Water Absorption at Saturation 0.030 %
0.030 %
Immersion; ASTM D570(2)
Mechanical Properties Metric English Comments
Hardness, Rockwell M 94
94
ASTM D785
Hardness, Rockwell R 125
125
ASTM D785
Hardness, Shore D 86
86
ASTM D2240
Tensile Strength 34.5 MPa
5000 psi
ASTM D638
Elongation at Break 1 %
1 %
ASTM D638
Tensile Modulus 5.03 GPa
730 ksi
ASTM D638
Flexural Strength 159 MPa
23000 psi
ASTM D790
Flexural Modulus 6.89 GPa
1000 ksi
ASTM D790
Compressive Strength 165 MPa
24000 psi
10% Def.; ASTM D695
Compressive Modulus 8.96 GPa
1300 ksi
ASTM D695
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256 Type A
Thermal Properties Metric English Comments
CTE, linear 45.0 µm/m-°C

@Temperature -40.0 - 149 °C
25.0 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Thermal Conductivity 0.303 W/m-K
2.10 BTU-in/hr-ft²-°F
ASTM F433
Melting Point 282 °C
540 °F
Crystalline, Peak; ASTM D3418
Maximum Service Temperature, Air 232 °C
450 °F
Long Term
Deflection Temperature at 1.8 MPa (264 psi) 254 °C
490 °F
ASTM D648
Flammability, UL94 V-0
V-0
1/8 inch (Estimated Rating)
Electrical Properties Metric English Comments
Surface Resistivity per Square >= 1.00e+13 ohm
>= 1.00e+13 ohm
EOS/ESD S11.11
Dielectric Strength 15.2 kV/mm
385 kV/in
Short Term; ASTM D149
Compliance Properties Metric English Comments
3A-Dairy No
No
Canada AG No
No
FDA No
No
NSF No
No
USDA No
No
USP Class VI No
No
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Limited
Limited
Acids, Weak Acceptable
Acceptable
Alcohols Acceptable
Acceptable
Alkalies, Strong (pH 11-14) Acceptable
Acceptable
Alkalies, Weak Acceptable
Acceptable
Chlorinated Solvents Acceptable
Acceptable
Conductive / Static Dissipative No
No
Continuous Sunlight Acceptable
Acceptable
Hot Water / Steam Acceptable
Acceptable
Hydrocarbons - Aliphatic Acceptable
Acceptable
Hydrocarbons - Aromatic Acceptable
Acceptable
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Acceptable
Acceptable
Descriptive Properties Value Comments
Machinability 7
1-10, 1=Easier to Machine
Users viewing this material also viewed the following: