Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ensinger TECATRON™ GF 40 Polyphenylene sulfide (PPS)

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS)
Manufacturer Ensinger
Trade Name TECATRON™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger TECATRON™ GF 40 Polyphenylene sulfide (PPS).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TECATRON PPS is a high performance thermoplastic that combines good mechanical properties with excellent thermal and chemical resistance properties. There is no known solvent that dissolves TECATRON PPS at temperatures below 392°F. Its low ionic impurities make it an excellent choice for applications where high purity is a concern. TECATRON GF40 is a glass reinforced material that offers extremely high strength along with excellent chemical resistance properties. TECATRON PVX is a bearing grade PPS that is suitable for high load applications.Information Provided by Ensinger Industries, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.64 g/cc
1.64 g/cc
ASTM D792
Density 1.64 g/cc
0.0592 lb/in³
ASTM D792
Water Absorption at Saturation 0.020 %
0.020 %
ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength at Break 184 MPa
26700 psi
Elongation at Break 1.9 %
1.9 %
ASTM D638
Tensile Modulus 14.0 GPa
2030 ksi
ASTM D638
Flexural Modulus 13.0 GPa
1890 ksi
ASTM D790
Thermal Properties Metric English Comments
CTE, linear 18.0 µm/m-°C
10.0 µin/in-°F
ASTM D696
Specific Heat Capacity 1.18 J/g-°C
0.282 BTU/lb-°F
Thermal Conductivity 0.251 W/m-K
1.74 BTU-in/hr-ft²-°F
Melting Point 282 °C
540 °F
ASTM D2133
Maximum Service Temperature, Air 230 °C
446 °F
Long Term
260 °C
500 °F
Intermittent
Deflection Temperature at 1.8 MPa (264 psi) 260 °C
500 °F
ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
ASTM D257
Surface Resistivity per Square 1.00e+15 ohm
1.00e+15 ohm
ASTM D257
Dielectric Constant 4.0
4.0
1 Mhz; ASTM D150
Dielectric Strength 20.0 kV/mm
508 kV/in
ASTM D149
Dissipation Factor 0.00010

@Temperature 22.8 °C
0.00010

@Temperature 73.0 °F
60 Hz; ASTM D150
0.0040
0.0040
1 Mhz; ASTM D150
Users viewing this material also viewed the following: