Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 78.0 °C | 172 °F | Exxon Method |
ExxonMobil Escorene® UL-7505 EVA Copolymer, Adhesive and Sealant Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 19.2% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants. |
|||
Melting Point | 78.0 °C | 172 °F | DSC |
DuPont™ Surlyn® 8120 Ionomer Resin, Sodium
(discontinued **) Surlyn® 8120 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu.. |
|||
Melting Point | 78.0 - 88.0 °C | 172 - 190 °F | |
Fine Organics FINALUX G 621 Lubricant Additive Applications: Compatible external lubricant with strong effet suitable for rigid PVC calendered films, fittings, bottles etc.Information provided by Fine Organics |
|||
Melting Point | 78.0 - 88.0 °C | 172 - 190 °F | |
Fine Organics FINAWAX E Lubricant Additive Applications: Slip additive for polyolefins, also suggested in artificial leather to achieve dry feel, release agent for plastisols.Information provided by Fine Organics |
|||
Melting Point | 77.9 °C | 172 °F | |
Indium Corp. GaCl3 Gallium Trichloride, Anhydrous Synonyms: Gallium Chloride, Gallium (III) ChlorideCAS Number: 13450-90-3EC Number: 236-610-0RTECS: LW9100000Purity: 99.5 to 99.999% Gallium TrichlorideAppearance: Clear or White, Needle-shaped.. |
|||
Melting Point | 78.0 °C | 172 °F | Eutectic |
Indium Corp. Indalloy 25 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 78.0 - 82.0 °C | 172 - 180 °F | RP-0304 |
Solvay ALKAMIDE® L-203 Surfactant Description: A solid lauramide monoethanolamide that readily disperses in hot water. Provides viscosity build, foam boosting and stabilization to shampoos and related cosmetic products.Chemical Name.. |
|||
Melting Point | 78.0 °C | 172 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Elvax® 3135X Ethylene-Vinyl Acetate Copolymer Resin for Thin Blown 12 wt% Vinyl Acetate.Elvax® 3135X is an extrudable, ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resi.. |
|||
Melting Point | 78.0 °C | 172 °F | Freezing Point; ASTM D3417 |
DuPont Elvax® 3135XZ Ethylene Vinyl Acetate DuPont™ Elvax® 3135XZ is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.Applicati.. |
|||
Melting Point | 78.0 °C | 172 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Nucrel® 3990 Ethylene-Acrylic Acid Copolymer Resin for Extrusion Coating/Laminating 9 wt% Acrylic Acid.Nucrel® 3990 is an ethylene-acrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment designed to .. |
|||
Melting Point | 78.0 °C | 172 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Nucrel® 0902HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film 9 wt% Methacrylic Acid.Nucrel® 0902HC (High-Clarity) is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment design.. |
|||
Melting Point | 77.8 °C | 172 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil Escorene® UL 7510 Adhesive Application Resin Escorene Ultra UL 7510 is a very high flow, 18.7% vinyl acetate copolymer that has very good compatibility with hydrocarbon tackifiers and most waxes. It is suitable for making hot melt adhesives, s.. |
|||
Melting Point | 78.0 °C | 172 °F | ASTM D3418, ISO 3146 |
DuPont™ HPF® 1000 Amorphous Polymer for Golf Balls DuPont™ HPF 1000 is extremely versatile and can be used to manufacture all layers of golf balls. DuPont™ HPF 1000 offers a combination of high resilience and low compression. This polymer is a hig.. |
|||
Melting Point | 78.0 °C | 172 °F | Freezing Point; ASTM D3418, ISO 3146 |
DuPont™ Nucrel® 3990L Ethylene Acrylic Acid Nucrel® 3990L is a copolymer of ethylene and acrylic acid. It is available for use in conventional extrusion coating, coextrusion coating and extrusion laminating equipment. 9.5 % By Weight Acrylic.. |
|||
Melting Point | 77.8 °C | 172 °F | Exxon Method |
ExxonMobil Optema® TC-110 Molding Ethylene Methyl Acrylate Product Description: Optema TC 110 is an ethylene methyl acrylate copolymer. TC 110 can be used for injection molding applications. It can be used in alloys, blends or compounds to increase impact s.. |
|||
Melting Point | 77.8 °C | 172 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil OPTEMA™ TC 120 ExCo Ethylene Methyl Acrylate Product Description: Optema TC 120 is an ethylene methyl acrylate copolymer intended for extrusion coating, coextrusion coating and extrusion lamination where good interlayer adhesion between polyet.. |
|||
Melting Point | 78.0 °C | 172 °F | DSC, 10°C/min; DuPont Test |
Dow Engage® 8003 Polyolefin Elastomer Description: Engage® 8003 polyolefin elastomer is an ethyleneoctene copolymer that has excellent flow characteristics and performs well in a wide variety of general purpose thermoplastic elastomer .. |
|||
Melting Point | 78.0 °C | 172 °F | DSC, 10°C/min; DuPont Test |
Dow Engage® 8401 Polyolefin Elastomer Description: Engage® 8401 polyolefin elastomer is an ethyleneoctene copolymer that offers excellent performance in durable, flexible injection molded industrial and consumer goods. Engage® 8401 pr.. |
|||
Melting Point | 78.0 °C | 172 °F | DSC |
Arkema Group LOTRYL® 30 BA 02 Copolymer Ethylene - Butyl Acrylate LOTRYL® 30 BA 02 is a random copolymer of ethylene and butyl acrylate, prepared by the high pressure polymerization process. LOTRYL® 30 BA 02 is used for polymer modification, in compounds formula.. |
|||
Melting Point | 78.0 °C | 172 °F | DSC |
Arkema Group EVATANE® 18-500 Copolymer Ethylene - Vinyl Acetate EVATANE® 18-500 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 18-500 is stabilized with antioxidants. The High Vinyl Acetate .. |