ExxonMobil Escorene® UL 7510 Adhesive Application Resin

Category Polymer , Adhesive , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
Manufacturer Exxon Chemical
Trade Name Escorene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene® UL 7510 Adhesive Application Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Escorene Ultra UL 7510 is a very high flow, 18.7% vinyl acetate copolymer that has very good compatibility with hydrocarbon tackifiers and most waxes. It is suitable for making hot melt adhesives, sealants and wax blends.Availability: Asia Pacific, Latin America, North America and South America Additive: Antiblock: NoSlip: NoThermal Stabilizer: Yes Applications:Adhesives and SealantsHot Melt AdhesivesIndustrial SealantsWax Blends Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.933 g/cc
0.0337 lb/in³
ExxonMobil Method
Vinyl Acetate Content 18.7 %
18.7 %
ExxonMobil Method
Melt Flow 500 g/10 min

@Load 2.16 kg,
Temperature 190 °C
500 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
15s; ASTM D2240
Hardness, Shore D 23
23
15s; ASTM D2240
Tensile Strength at Break 2.90 MPa
420 psi
ASTM D638
Elongation at Break 330 %
330 %
ASTM D638
Flexural Modulus 0.0372 GPa
5.40 ksi
1% secant; ASTM D790
Thermal Properties Metric English Comments
Melting Point 77.8 °C
172 °F
Peak Melting Temperature; ExxonMobil Method