Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 78.0 °C | 172 °F | Exxon Method |
ExxonMobil Escorene® UL-7505 EVA Copolymer, Adhesive and Sealant Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 19.2% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants. |
|||
Melting Point | 78.0 °C | 172 °F | DSC |
DuPont™ Surlyn® 8120 Ionomer Resin, Sodium
(discontinued **) Surlyn® 8120 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu.. |
|||
Melting Point | 78.0 - 88.0 °C | 172 - 190 °F | |
Fine Organics FINALUX G 621 Lubricant Additive Applications: Compatible external lubricant with strong effet suitable for rigid PVC calendered films, fittings, bottles etc.Information provided by Fine Organics |
|||
Melting Point | 78.0 - 88.0 °C | 172 - 190 °F | |
Fine Organics FINAWAX E Lubricant Additive Applications: Slip additive for polyolefins, also suggested in artificial leather to achieve dry feel, release agent for plastisols.Information provided by Fine Organics |
|||
Melting Point | 78.0 °C | 172 °F | Eutectic |
Indium Corp. Indalloy 25 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 78.0 - 82.0 °C | 172 - 180 °F | RP-0304 |
Solvay ALKAMIDE® L-203 Surfactant Description: A solid lauramide monoethanolamide that readily disperses in hot water. Provides viscosity build, foam boosting and stabilization to shampoos and related cosmetic products.Chemical Name.. |
|||
Melting Point | 78.0 °C | 172 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Elvax® 3135X Ethylene-Vinyl Acetate Copolymer Resin for Thin Blown 12 wt% Vinyl Acetate.Elvax® 3135X is an extrudable, ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resi.. |
|||
Melting Point | 78.0 °C | 172 °F | Freezing Point; ASTM D3417 |
DuPont Elvax® 3135XZ Ethylene Vinyl Acetate DuPont™ Elvax® 3135XZ is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.Applicati.. |
|||
Melting Point | 78.0 °C | 172 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Nucrel® 3990 Ethylene-Acrylic Acid Copolymer Resin for Extrusion Coating/Laminating 9 wt% Acrylic Acid.Nucrel® 3990 is an ethylene-acrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment designed to .. |
|||
Melting Point | 78.0 °C | 172 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Nucrel® 0902HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film 9 wt% Methacrylic Acid.Nucrel® 0902HC (High-Clarity) is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment design.. |
|||
Melting Point | 78.0 °C | 172 °F | ASTM D3418, ISO 3146 |
DuPont™ HPF® 1000 Amorphous Polymer for Golf Balls DuPont™ HPF 1000 is extremely versatile and can be used to manufacture all layers of golf balls. DuPont™ HPF 1000 offers a combination of high resilience and low compression. This polymer is a hig.. |
|||
Melting Point | 78.0 °C | 172 °F | Freezing Point; ASTM D3418, ISO 3146 |
DuPont™ Nucrel® 3990L Ethylene Acrylic Acid Nucrel® 3990L is a copolymer of ethylene and acrylic acid. It is available for use in conventional extrusion coating, coextrusion coating and extrusion laminating equipment. 9.5 % By Weight Acrylic.. |
|||
Melting Point | 78.0 °C | 172 °F | DSC, 10°C/min; DuPont Test |
Dow Engage® 8003 Polyolefin Elastomer Description: Engage® 8003 polyolefin elastomer is an ethyleneoctene copolymer that has excellent flow characteristics and performs well in a wide variety of general purpose thermoplastic elastomer .. |
|||
Melting Point | 78.0 °C | 172 °F | DSC, 10°C/min; DuPont Test |
Dow Engage® 8401 Polyolefin Elastomer Description: Engage® 8401 polyolefin elastomer is an ethyleneoctene copolymer that offers excellent performance in durable, flexible injection molded industrial and consumer goods. Engage® 8401 pr.. |
|||
Melting Point | 78.0 °C | 172 °F | DSC |
Arkema Group LOTRYL® 30 BA 02 Copolymer Ethylene - Butyl Acrylate LOTRYL® 30 BA 02 is a random copolymer of ethylene and butyl acrylate, prepared by the high pressure polymerization process. LOTRYL® 30 BA 02 is used for polymer modification, in compounds formula.. |
|||
Melting Point | 78.0 °C | 172 °F | DSC |
Arkema Group EVATANE® 18-500 Copolymer Ethylene - Vinyl Acetate EVATANE® 18-500 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 18-500 is stabilized with antioxidants. The High Vinyl Acetate .. |