Fine Organics FINAWAX E Lubricant Additive

Category Fluid , Lubricant , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Fine Organics
Trade Name FINAWAX
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fine Organics FINAWAX E Lubricant Additive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Slip additive for polyolefins, also suggested in artificial leather to achieve dry feel, release agent for plastisols.Information provided by Fine Organics
Physical Properties Metric English Comments
Additive Loading 0.20 - 0.50 %
0.20 - 0.50 %
P PVC
Thermal Properties Metric English Comments
Melting Point 78.0 - 88.0 °C
172 - 190 °F
Descriptive Properties Value Comments
Influence on Transparency Opaque
Lubricating Effect External
Physical Form Solid