ExxonMobil Optema® TC-110 Molding Ethylene Methyl Acrylate

Category Polymer , Thermoplastic , Ethylene Methyl Acrylate , Ethylene-Methyl Acrylate Copolymer, Compounding Grade
Manufacturer Exxon Chemical
Trade Name Optema®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Optema® TC-110 Molding Ethylene Methyl Acrylate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Optema TC 110 is an ethylene methyl acrylate copolymer. TC 110 can be used for injection molding applications. It can be used in alloys, blends or compounds to increase impact strength or to lower the modulus. TC 110 can be injection molded and extruded. Availability: Latin America, North America and South America Additive: Thermal Stabilizer: YesApplications: CompatibilizerEngineering thermoplastic impact modifierFoamsInjection MoldingSoft, molded partsData provided by the manufacturer, Exxon Chemical.
Physical Properties Metric English Comments
Density 0.942 g/cc
0.0340 lb/in³
Exxon Method
Methyl Acrylate Content 21.5 %
21.5 %
Exxon Method
Melt Flow 2.00 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.00 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Exxon Method
Mechanical Properties Metric English Comments
Hardness, Shore A 86

@Time 15.0 sec
86

@Time 0.00417 hour
ASTM D2240
Hardness, Shore D 26

@Time 15.0 sec
26

@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break 8.27 MPa
1200 psi
ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Flexural Modulus, 1% Secant 37.2 MPa
5400 psi
ASTM D790
Dart Drop, Total Energy 17.6 J

@Temperature 22.8 °C
13.0 ft-lb

@Temperature 73.0 °F
ASTM D3763
32.5 J

@Temperature -40.0 °C
24.0 ft-lb

@Temperature -40.0 °F
ASTM D3763
Thermal Properties Metric English Comments
Melting Point 77.8 °C
172 °F
Exxon Method
Vicat Softening Point 51.1 °C
124 °F
Peak Melting Temperature; ASTM D1525