Material Notes:
DuPont™ HPF 1000 is extremely versatile and can be used to manufacture all layers of golf balls. DuPont™ HPF 1000 offers a combination of high resilience and low compression. This polymer is a highly amorphous material. Used in golf ball construction
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
ASTM D792, ISO 1183
Melt Flow 0.65 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.65 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 52
52
ASTM D2240
Tensile Strength 18.0 MPa
2610 psi
ASTM D638
Elongation at Break 430 %
430 %
ASTM D638
Flexural Modulus 0.220 GPa
31.9 ksi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 78.0 °C
172 °F
ASTM D3418, ISO 3146
Vicat Softening Point 59.0 °C
138 °F
ASTM D1525, ISO 306
Processing Properties Metric English Comments
Processing Temperature <= 285 °C
<= 545 °F