ExxonMobil Escorene® UL-7505 EVA Copolymer, Adhesive and Sealant Grade  (discontinued **)

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene® UL-7505 EVA Copolymer, Adhesive and Sealant Grade  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Exxon Chemical.A 19.2% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants.
Physical Properties Metric English Comments
Density 0.947 g/cc
0.0342 lb/in³
Exxon Method
Apparent Bulk Density 0.540 g/cc
0.0195 lb/in³
ASTM D1895 (B)
Viscosity 300 cP

@Temperature 121 °C
300 cP

@Temperature 250 °F
melt viscosity; ASTM D-3236
Melt Flow 600 g/10 min
600 g/10 min
Exxon Method
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
ASTM D2240
Tensile Strength, Ultimate 3.40 MPa
493 psi
ASTM D638
Elongation at Break 140 %
140 %
ASTM D638
Thermal Properties Metric English Comments
Melting Point 78.0 °C
172 °F
Exxon Method
Vicat Softening Point 89.0 °C
192 °F
Softening Point, R&B; ASTM E-28