Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene® LL-3201 LLDPE/Hexene Premium High Strength 0.6 mil Film, Stiff  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Exxon Chemical.An LLDPE hexene copolymer film resin. Films made from this resin have outstanding tensile, stiffness and toughness properties. These superior properties along with the resin's good drawdown capability permit usage in many demanding packaging applicationsApplications: Grocery sacks; Merchandise bags; Frozen food packaging; Heavy duty bags; Stretch film. Data for film properties below based on 0.6 mil film.
Physical Properties Metric English Comments
Density 0.925 g/cc
0.0334 lb/in³
Exxon Method
Thickness 15.2 microns
0.600 mil
Melt Flow 0.80 g/10 min
0.80 g/10 min
Exxon Method
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 12.4 MPa
1800 psi
ASTM D882
Film Tensile Strength at Yield, TD 13.7 MPa
1990 psi
ASTM D882
Film Elongation at Break, MD 480 %
480 %
ASTM D882
Film Elongation at Break, TD 730 %
730 %
ASTM D882
Secant Modulus, MD 0.262 GPa
38.0 ksi
ASTM D882
Secant Modulus, TD 0.324 GPa
47.0 ksi
ASTM D882
Elmendorf Tear Strength MD 80 g
80 g
ASTM D1922
Elmendorf Tear Strength TD 640 g
640 g
ASTM D1922
Elmendorf Tear Strength, MD 5.24 g/micron
133 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 42.01 g/micron
1067 g/mil
ASTM D1922
Dart Drop 5.24 g/micron
133 g/mil
F50; ASTM D1709
Dart Drop Test 80.0 g
0.176 lb
F50; ASTM D-1709
Film Tensile Strength at Break, MD 66.2 MPa
9600 psi
ASTM D882
Film Tensile Strength at Break, TD 46.9 MPa
6800 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point 124 °C
255 °F
Exxon Method
Optical Properties Metric English Comments
Haze 11 %
11 %
ASTM D1003
Gloss 50 %
50 %
45°, ASTM D-2457