Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NOVA Chemicals Sclair® 94E Butene LMDPE Film and Extrusion Resin

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , MDPE , Linear Medium Density Polyethylene (LMDPE), Film
Manufacturer NOVA Chemicals
Trade Name Sclair®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Sclair® 94E Butene LMDPE Film and Extrusion Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Excellent processabilityGood stiffness and strengthHigh stretchability Applications: Overwrap filmNettingBlend resinInformation provided by Nova Chemicals
Physical Properties Metric English Comments
Density 0.936 g/cc
0.0338 lb/in³
ASTM D792
Thickness 25.0 microns
0.984 mil
Melt Flow 1.8 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.8 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ASTM D2240
Tensile Strength at Break 30.0 MPa
4350 psi
ASTM D638
Tensile Strength, Yield 17.2 MPa
2500 psi
ASTM D638
Elongation at Break 1100 %
1100 %
ASTM D638
Puncture Energy 0.275 J
0.203 ft-lb
Low Friction Puncture
Elmendorf Tear Strength MD 19 g
19 g
ASTM D1922
Elmendorf Tear Strength TD 140 g
140 g
ASTM D1922
Dart Drop Test 40.0 g
0.0882 lb
ASTM D1709/A
Thermal Properties Metric English Comments
Melting Point 124 °C
255 °F
NOVA
Vicat Softening Point 119 °C
246 °F
ASTM D1525
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D746