Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeri Europa Flexirene® MR 56 A Linear Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Injection Molded
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Flexirene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Flexirene® MR 56 A Linear Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flexirene MR 56 A is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Parts made with Flexirene MR 50 A are characterized by optimum rigidity. Flexirene MR 56 A is highly pure and it is suitable for all application where organoleptic properties are required.
Physical Properties Metric English Comments
Specific Gravity 0.939 g/cc
0.939 g/cc
ISO 1183
Melt Flow 22 g/10 min

@Load 2.16 kg,
Temperature 190 °C
22 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 56
56
ISO 868/A
Tensile Strength at Break 15.0 MPa
2180 psi
ISO 527
Tensile Strength, Yield 15.0 MPa
2180 psi
ISO 527
Elongation at Break >= 500 %
>= 500 %
ISO 527
Flexural Modulus 0.500 GPa
72.5 ksi
ISO 178
Thermal Properties Metric English Comments
Melting Point 124 °C
255 °F
Internal method
Vicat Softening Point 112 °C

@Load 1.00 kg
234 °F

@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D746