Lubrizol ESTANE® 58271 Ester Based Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Polyester Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol ESTANE® 58271 Ester Based Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Good physical properties, chemical resistance and adhesive properties and wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and blow molding.Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Maximum Moisture Content 0.020
0.020
Mechanical Properties Metric English Comments
Hardness, Shore A 82 - 88

@Time 5.00 sec
82 - 88

@Time 0.00139 hour
ASTM D2240
Tensile Strength 51.7 MPa
7500 psi
ASTM D412
Elongation at Break 550 %
550 %
ASTM D412
100% Modulus 0.00550 GPa
0.798 ksi
ASTM D412
300% Modulus 0.00970 GPa
1.41 ksi
ASTM D412
Tear Strength 22.8 kN/m
130 pli
Trouser; ASTM D470
Graves Tear Strength 78.9 kN/m
450 pli
DieC; ASTM D624
Taber Abrasion, mg/1000 Cycles 2.5
2.5
H18, 1000g; ASTM D3389 B
Tensile Set 13 %
13 %
200% elongation; ASTM D412
Thermal Properties Metric English Comments
Melting Point 115 °C
239 °F
Kofler
120 °C
248 °F
DSC
Glass Transition Temp, Tg -28.0 °C
-18.4 °F
DSC
Optical Properties Metric English Comments
Haze 1.1 %
1.1 %
65 mil between glass; ASTM D-1003
Processing Properties Metric English Comments
Zone 1 177 °C
351 °F
Extrusion
Zone 2 182 °C
360 °F
Extrusion
Zone 3 188 °C
370 °F
Extrusion
Zone 4 193 °C
379 °F
Extrusion
Adapter Temperature 193 °C
379 °F
5, Extrusion
Die Temperature 193 °C
379 °F
Zone 1, 6, Extrusion
193 °C
379 °F
Zone 2, Extrusion
Drying Temperature 104 °C
219 °F
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Dew Point -40.0 °C
-40.0 °F