Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 140 - 152 °C | 284 - 306 °F | |
Indium Corp. Indalloy 230 Indium-Tin-Lead Solder Alloy Also known as 532Information Provided by Indium Corporation |
|||
Melting Point | 140 - 152 °C | 284 - 306 °F | |
Indium Corp. Indalloy 532 Tin Solder Alloy Also known as 230Information Provided by Indium Corporation |
|||
Melting Point | 120 - 152 °C | 248 - 306 °F | |
Indium Corp. Indalloy 89 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 148 - 152 °C | 298 - 306 °F | |
Arkema Group KYNAR® LBG1 Polyvinylidene Fluoride Powder Characteristics: White, non-hygroscopic powder.Applications: Membrane, Lithium ion battery applicationsInformation provided by Arkema Inc. |