Thermal Properties Metric English Comments
Melting Point 125 - 130 °C
257 - 266 °F
Polimersan Plastics POLIPOLEN® (Polyethylene) HD-PE 300
PE 300: Polyethylene with high density. POLIPOLEN® PE (POLYETHYLENE) is maintained from coke oven gas or from natural gas or from Ethene or Ethane which is produced by cracking of petroleum. Monom..
Melting Point 125 - 130 °C
257 - 266 °F
Polimersan Plastics POLIPOLEN® (Polyethylene) HD-PE 300
PE 300: Polyethylene with high density. POLIPOLEN® PE (POLYETHYLENE) is maintained from coke oven gas or from natural gas or from Ethene or Ethane which is produced by cracking of petroleum. Monom..
Melting Point -80.0 - 130 °C
-112 - 266 °F
Average value: 40.0 °C Grade Count:4
Overview of materials for Epoxy Cure Resin
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate M..
Melting Point 110 - 130 °C
230 - 266 °F
0.025" extruded film,
Huntsman IROGRAN® PS455-200 TPU-Polyester
Introduction: IROGRAN PS455-200 is a polyester based thermoplastic polyurethane intended for extrusion applications. IROGRAN PS455-200 is part of the HUNTSMAN film and sheet product range and offers..
Melting Point 121 - 130 °C
250 - 266 °F
Indium Corp. Indalloy 70 Indium-Tin Solder Alloy
Information Provided by Indium Corporation
Melting Point 110 - 130 °C
230 - 266 °F
LG Chemical LUTENE XL2700BK PE Compound
Description: LUTENE XL2700BK has excellent strippability, processability, weather resistance, heat resistance for medium and high voltage power cables. The advantage of LUTENE XL2700BK over conventi..
Melting Point 120 - 130 °C
248 - 266 °F
LG Chemical LUTENE XL8080NT PE Compound
Description: LUTENE XL8080NT is a standard version having excellent electrical properties for medium and high voltage power cable insulation and has a very low level of contamination.Applications: M..
Melting Point 60.0 - 130 °C
140 - 266 °F
Lucobit Lucowax® 1700 Polyethylene Wax
Lucowax is a polyethylene wax additive for the modification of bitumen or asphalt.The addition of Lucowax reduces viscosity and penetration, while increasing water resistance, plasticity, and deform..
Melting Point 100 - 130 °C
212 - 266 °F
LG Chemical LUTENE CCO550BK PE Compound
Description: LUTENE CC0550BK offer the following properties: high mechanical properties, good environmental stress cracking resistance, excellent wetherability and high speed extrusion to give a smo..
Melting Point 120 - 130 °C
248 - 266 °F
LG Chemical LUTENE XL8080UC PE Compound
Description: LUTENE XL8080UC is a superior cleanliness version for high voltage power cable insulation and is designated as UC (Ultra-Clean) due to its extremely low level of contamination. LUTENE X..
Melting Point 120 - 130 °C
248 - 266 °F
DSC
EMS-Griltech Griltex® 2A Copolyamide Hotmelt Adhesive (Apparel Interlinings)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Melting Point 120 - 130 °C
248 - 266 °F
DSC
EMS-Griltech Griltex® 2A Copolyamide Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Melting Point 125 - 130 °C
257 - 266 °F
DSC
EMS-Griltech Griltex® 6E Copolyester Hotmelt Adhesive (Apparel Interlinings)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Melting Point 125 - 130 °C
257 - 266 °F
DSC
EMS-Griltech Griltex® 6E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Melting Point 120 - 130 °C
248 - 266 °F
DSC
EMS-Griltech Griltex® D 1439E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Melting Point 120 - 130 °C
248 - 266 °F
DSC
EMS-Griltech Griltex® D 1441E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Melting Point 120 - 130 °C
248 - 266 °F
DSC
EMS-Griltech Griltex® D 1519E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Melting Point 125 - 130 °C
257 - 266 °F
BASF NEOL® Neolpentylglycol Flakes
Formula: C5H12O2CAS: 126-30-7Description: Neolpentylglycol (NEOL) flakes are colorless with a sweetish odor.Synonyms: Neopentanediol, 2,2-Dimethyl-1,3-propanediol, 1,3-Dihydroxy-2,2-dimethylpropane,..
Melting Point 125 - 130 °C
257 - 266 °F
BASF NEOL® Neolpentylglycol Pure Liquid
Formula: C5H12O2CAS: 126-30-7Description: Neolpentylglycol (NEOL) pure liquid is a colorless melt, with a sweetish odor. Synonyms: Neopentanediol, 2,2-Dimethyl-1,3-propanediol, 1,3-Dihydroxy-2,2-dim..
Melting Point 116 - 130 °C
241 - 266 °F
Average value: 123 °C Grade Count:57
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum ..