Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 120 - 125 °C | 248 - 257 °F | |
Oceanchem Group 2,2-Dibromo-3-nitrilopropionamide (DBNPA) Molecular Formula: C3H2Br2N2OCas No.: 10222-01-2Features: DBNPA is white crystal powder, may dissolve in acetone, polyethylene glycol, benzene, ethanol, etc, organic solvent, slightly dissolved in w.. |
|||
Melting Point | 85.0 - 125 °C | 185 - 257 °F | |
S&E Specialty Polymers GPE2001E-ROHS PVC GPE2001E-ROHS flame retardant polyethylene compound designed for wire and cable applications. GPE2001E-ROHS complies with RoHS requirements. GPE2001E-ROHS is suitable for 75°C continuous use and 10.. |
|||
Melting Point | 85.0 - 125 °C | 185 - 257 °F | |
S&E Specialty Polymers GPE2001F-ROHS PVC Application: GPE2001F-ROHS is flame retardant polyethylene compound designed for wire and cable applications. GPE2001F-ROHS complies with RoHS requirements. GPE2001F-ROHS is suitable for 75°C cont.. |
|||
Melting Point | 110 - 125 °C | 230 - 257 °F | |
Hong Kun Group AO 1010 Antioxidant CAS No. 6683-19-8All information provided by Hongkun Group |
|||
Melting Point | 118 - 125 °C | 244 - 257 °F | |
Indium Corp. Indalloy 1 Indium-Tin Solder Alloy Fair wettability on glass, quartz, and many ceramics. Good low temperature malleability. Compensates for some CTE mismatch. Low vapor pressureInformation Provided by Indium Corporation |
|||
Melting Point | 110 - 125 °C | 230 - 257 °F | |
Suqian Unitechem Antioxidant 1010 Chemical Name: Tetrakis [methylene-3-(3,5-di-tert-butyl-4-hydroxyphenyl-propionate)]methaneCAS NO.: 6683-19-8Molecular Formula: C73H108O12Properties: The product takes on the appearance of white pow.. |
|||
Melting Point | 115 - 125 °C | 239 - 257 °F | DSC |
EMS-Griltech Griltex® D 1541A Copolyamide Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melting Point | 115 - 125 °C | 239 - 257 °F | DSC |
EMS-Griltech Griltex® D 1566A Heat Stabilized Copolyamide Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melting Point | 117 - 125 °C | 243 - 257 °F | |
Arkema Group KYNAR FLEX® 2500-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Highest flexibility. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical st.. |
|||
Melting Point | 117 - 125 °C | 243 - 257 °F | |
Arkema Group KYNAR® 2501-20 Polyvinylidene Fluoride Powder Characteristics: White, non-hygroscopic powder. Very flexible, very soluble. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low p.. |