Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 9.16 g/cc
0.331 lb/in³
Thermal Properties Metric English Comments
Melting Point 120 - 152 °C
248 - 306 °F
Solidus 120 °C
248 °F
Liquidus 152 °C
306 °F
Component Elements Properties Metric English Comments
Bismuth, Bi 21 %
21 %
Lead, Pb 42 %
42 %
Tin, Sn 37 %
37 %