Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chesterton 615 High Temperature Grease

Category Fluid , Lubricant
Manufacturer Chesterton
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chesterton 615 High Temperature Grease.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Chesterton® 615 High Temperature Grease is the one grease to use for the most demanding of lubrication needs. It is a multi-purpose workhorse with outstanding extreme pressure capabilities. With a temperature limit of 204°C, it performs at temperatures well beyond that of most conventional petroleum greases. The product is compatible with most other popular greases, has outstanding shear resistance and excellent corrosion resistance. Even when up to 50% water is incorporated into the product, the grease maintains its protective film and can withstand extremes of pressure. Uses for Chesterton 615 High Temperature Grease can be found throughout any industrial plant. It is especially advantageous where there is a high water environment such as in a pulp and paper mill, extremes of pressure such as in mining, or extremes of temperature such as in steel mills.Features:Excellent for extremes of pressure and temperatureSuperior resistance to water washoutExceptional shear resistanceOxidation inhibitedContains no toxic heavy metalsCompatible with most popular greasesNSF H2 - Registration number 133940. ISO L-XCDIB2DIN 51 502-KPF 2P-30.Applications: Use in any industrial plant where operating conditions subject a lubricant to extremes of heat and pressure. Examples of industries using Chesterton 615 High Temperature Grease are the steel, pulp and paper, mining, transportation, coal and ore processing, construction, metal fabrication and marine industries. Applications range from the lubrication of conveyors, grinding mills, crushers, bearings, shears, blowers, rolling mills, traveling cranes, mechanical presses, cams, toggle joints, guides, ways, slides to any industrial and marine machines an equipment subject to extremes of temperature and pressureInformation provided by Chesterton
Physical Properties Metric English Comments
Specific Gravity 0.970 g/cc
0.970 g/cc
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Load Wear Index 85
85
ASTM D2596, DIN 51 350/4
Four Ball Extreme Pressure, Weld Load 620 kg
1370 lb (mass)
ASTM D2596, DIN 51 350/4
Four Ball Wear 0.400 mm
0.0157 in
Scar Diameter; ASTM D2266, DIN 51 350/5
Penetration 265 - 295
265 - 295
ASTM D217, DIN ISO 2137
Oil Separation 0.20 %
0.20 %
loss; ASTM D1742
Timken Test 29500 g
65.0 lb
OK Load; ASTM D2509
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
399 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Dropping Point 318 °C
604 °F
ASTM D2265, DIN 51 801/1
Descriptive Properties Value Comments
Bearing Life 120 hours
Wheel, ASTM D3527
Color Blue-Green
Consistency 2
NLGI, DIN 51 818
Corrosion Resistance >1000 hrs
@ 50 microns film thickness, 5% NaCl, ASTM B117
Shear Stability +2%
10000 strokes, ASTM D217
+4%
100000 strokes, ASTM D217
Texture Buttery with slight tack
Water Washout Resistance <0.05%
ASTM D1264