Material Notes:
Red Nitrile Butadiene / PVC elastomer blend 59-65°IRHD. Electrically non-conductive. Copolymer of acrylonitrile and butadiene, blended with polyvinyl chloride.Applications: Specially formulated as a non-conductive, soft and flexible rubber for the manufacture of electrical cable terminal covers. Excellent resistance against petroleum and mineral based fuels and oils. The addition of PVC provides improved resistance to ozone.
Mechanical Properties Metric English Comments
Hardness, Shore A 62
62
°IRHD; ASTM D1415
69
69
°IRHD, +7 change after 240 hours @ 70°C; ASTM D1415
Tensile Strength, Yield 9.00 MPa
1310 psi
-10% change after 240 hours @ 70°C; ASTM D412
10.0 MPa
1450 psi
ASTM D412
Elongation at Break 210 %
210 %
-25% change after 240 hours @ 70°C; ASTM D412
280 %
280 %
ASTM D412
Compression Set 45 %
45 %
24 hours @ 100°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 120 °C
248 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
-10.0 °C
14.0 °F
T10
Flash Point >= 300 °C
>= 572 °F