Precision Polymer Engineering B60B Styrene Butadiene Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering B60B Styrene Butadiene Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Styrene-Butadiene Rubber (SBR) 55-65 °IRHD. Copolymer of styrene and butadiene.Applications: Good sealing resistance to brake fluids and water. Poor against petroleum oils, solvents and weather. The use of SBR in automotive brake systems has now been superseded by EPDM.
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
°IRHD; ASTM D1415
63
63
°IRHD, +3 change after 72 hours @ 70°C; ASTM D1415
Tensile Strength, Yield 9.94 MPa
1440 psi
-29% change after 72 hours @ 70°C; ASTM D412
14.0 MPa
2030 psi
ASTM D412
Elongation at Break 400 %
400 %
ASTM D412
488 %
488 %
22% change after 72 hours @ 70°C; ASTM D412
Compression Set 30 %
30 %
24 hours @ 70°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 °C
212 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Flash Point >= 200 °C
>= 392 °F