Material Notes:
Peroxide Cured, Nitrile Butadiene Rubber (NBR), 55-65 °IRHD. Copolymer of acrylonitrile and butadiene. Formulated using only those ingredients determined by the United States Food and Drug Administration (FDA) to be in accordance with Code of Federal Regulations Title 21 (CFR21), Section 177.2600.Applications: Formulation designed for repeated use in equipment associated with the production of foodstuffs intended for human consumption.
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
°IRHD; ASTM D1415
75
75
°IRHD, +15 change after 70 hours @ 100°C; ASTM D1415
Tensile Strength, Yield 11.2 MPa
1620 psi
-20% change after 70 hours @ 100°C; ASTM D412
14.0 MPa
2030 psi
ASTM D412
Elongation at Break 180 %
180 %
-40% change after 70 hours @ 100°C; ASTM D412
300 %
300 %
ASTM D412
Compression Set 25 %
25 %
24 hours @ 100°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 120 °C
248 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
-40.0 °C
-40.0 °F
Non-brittle after 3 minutes
Flash Point >= 300 °C
>= 572 °F