Material Notes:
General purpose, peroxide cured, Ethylene Propylene Terpolymer, 70-75 °IRHD. Terpolymer of ethylene, propylene and diene monomers. To meet ASTM D2000/SAE J200 line call-out M5CA710, A25, B35, C32, EA14, F17.Applications: Excellent water and steam resistance with good compression set properties. Better heat and chemical resistance than sulphur cured EPDM. Not mineral oil resistant.
Mechanical Properties Metric English Comments
Hardness, Shore A 74
74
°IRHD; ASTM D1415
77
77
°IRHD, +3 change after 70 hours @ 100°C; ASTM D1415
Tensile Strength, Yield 14.454 MPa
2096.4 psi
-1% change after 70 hours @ 100°C; ASTM D412
14.6 MPa
2120 psi
ASTM D412
Elongation at Break 179.78 %
179.78 %
-11% change after 70 hours @ 100°C; ASTM D412
202 %
202 %
ASTM D412
Compression Set 5.0 %
5.0 %
24 hours @ 125°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 125 °C
257 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Flash Point >= 200 °C
>= 392 °F
Users viewing this material also viewed the following: