Fainplast Compounds RI 55 Rigid PVC, Injection Molding

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Fainplast Compounds
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds RI 55 Rigid PVC, Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fittings for building trade - high fluidity
Physical Properties Metric English Comments
Density 1.43 - 1.47 g/cc
0.0517 - 0.0531 lb/in³
ISO R 1184
Mechanical Properties Metric English Comments
Tensile Strength at Break 36.0 MPa
5220 psi
ISO R 527
Tensile Strength, Yield 40.0 MPa
5800 psi
ISO R527
Elongation at Break 110 %
110 %
ISO R 527
Izod Impact, Unnotched 0.400 - 0.800 J/cm

@Temperature 23.0 °C
0.749 - 1.50 ft-lb/in

@Temperature 73.4 °F
ISO R180
Thermal Properties Metric English Comments
Vicat Softening Point 79.0 - 81.0 °C

@Load 5.00 kg
174 - 178 °F

@Load 11.0 lb
ISO R306