Dow AFFINITY™ SM 1300G Polyolefin Plastomer (POP)

Category Polymer , Thermoplastic , Polyolefin
Manufacturer Dow Chemical
Trade Name AFFINITY™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow AFFINITY™ SM 1300G Polyolefin Plastomer (POP).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AFFINITY™ SM 1300G is an ethylene alpha-olefin resin for Injection Molding is produced via INSITE™ Technology from Dow Plastics. The resin offers excellent performance in durable injection molded industrial and consumer goods and compression molded closure liners or gaskets.Information provided by Dow
Physical Properties Metric English Comments
Density 0.902 g/cc
0.0326 lb/in³
ASTM D792
Thickness 3180 microns
125 mil
injection molded
Melt Flow 30 g/10 min
30 g/10 min
ASTM D1238
Slip Level 600 ppm
600 ppm
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 9.142 MPa
1326 psi
crosshead speed 20 in./min; ASTM D638
Tensile Strength, Yield 4.12 MPa
598 psi
crosshead speed 20 in./min; ASTM D638
Elongation at Break 624 %
624 %
crosshead speed 20 in./min; ASTM D638
Flexural Modulus 0.07088 GPa
10.28 ksi
ASTM D790
2% Secant Modulus 0.07088 GPa
10.28 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm

@Temperature -50.0 °C
1.00 ft-lb/in

@Temperature -58.0 °F
ASTM D256
2.14 J/cm

@Temperature 23.0 °C
4.00 ft-lb/in

@Temperature 73.4 °F
ASTM D256
2.67 J/cm

@Temperature 0.000 °C
5.00 ft-lb/in

@Temperature 32.0 °F
ASTM D256
4.81 J/cm

@Temperature -20.0 °C
9.00 ft-lb/in

@Temperature -4.00 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 98.0 °C
208 °F
Dow Method (DSC)
Vicat Softening Point 79.0 °C
174 °F
ASTM D1525