Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 79.0 - 182 °C | 174 - 360 °F | Average value: 136 °C Grade Count:6 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Glass Filled". Each property range of values reported is minimum .. |