Karina 837-10/119-E-ERYB White PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina 837-10/119-E-ERYB White PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.52 - 1.58 g/cc
1.52 - 1.58 g/cc
ASTM D 792
ASTM Color -3.90 - -2.30
-3.90 - -2.30
Color B, ME 12
-1.57 - 0.030
-1.57 - 0.030
Color A, ME 12
89.11 - 90.71
89.11 - 90.71
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore D 78 - 82

@Time 15.0 sec
78 - 82

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 31.4 MPa
>= 4550 psi
ASTM D 638
Thermal Properties Metric English Comments
Vicat Softening Point >= 79.0 °C
>= 174 °F
ASTM D 1525
Heat Distortion Temperature >= 76.0 °C
>= 169 °F
ASTM D 648
Descriptive Properties Value Comments
Application General Purpose Profiles