Polymer Property : Vicat Softening Point = 120 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 49.0 °C
120 °F
Rate A; ASTM D1525
Covestro Texin® DP7-3008 Thermoplastic Polyurethane, Polyester-based, Aliphatic  (discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
Vicat Softening Point 49.0 °C
120 °F
ASTM D1525
ICO Polymers ICOFLOâ„¢ 510-5003 1000 Micron EVA Powder
Description: ICOFLO 510-5003 is an EVA powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in masterbatch (inste..
Vicat Softening Point 49.0 °C
120 °F
ASTM D1525
ICO Polymers ICOTEXâ„¢ 520-5076 500 Micron EVA Powder
Description: ICOTEX 520-5076 is an EVA powder that has been developed to meet the special requirements of the textile coating industry. Its key characteristics are a good melt flow and flexibility,..
Vicat Softening Point 48.9 °C
120 °F
Loading 2 (50N); ASTM D1525
Teknor Apex Sinvicomp SHM 2432 Polyvinyl Chloride, Flexible
Availability: Asia Pacific Features: Ethylene Oxide Sterilizable Uses: Medical/Healthcare Applications Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex
Vicat Softening Point 49.0 °C
120 °F
ASTM D1525
DuPont Elvax® 265 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
Vicat Softening Point 49.0 °C
120 °F
ASTM D1525
DuPont Elvax® 3182 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion
28 wt% Vinyl Acetate.Elvax® 3182-2 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resi..
Vicat Softening Point 49.0 °C
120 °F
ASTM D1525, ISO 306
DuPont Elvax® 3182-2 Ethylene Vinyl Acetate
DuPont™ Elvax® 3182-2 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. Applicat..
Vicat Softening Point 49.0 °C
120 °F
ASTM D1525
DuPont Bynel® 1124 Modified EVA Adhesive Resin
Bynel® Series 1100 resins are modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylen..
Vicat Softening Point 48.9 °C
120 °F
ASTM D1525
ExxonMobil Escorene® LD 768.MJ Molding, extrusion and compounding resin
Escorene Ultra LD 768.MJ is a high viscosity, 26.2% vinyl acetate copolymer suitable for making very soft, blow molded or extruded articles with very good low temperature toughness. It can also be ..
Vicat Softening Point 49.0 °C
120 °F
ASTM D1525, ISO 306
DuPont™ Elvax® 3190A Ethylene Vinyl Acetate
DuPont™ Elvax® 3190A is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. ELVAX® 3..
Vicat Softening Point 48.9 °C
120 °F
ASTM D1525
Dow AMPLIFY™ EA 103 Ethylene-ethyl Acrylate (EEA)
AMPLIFY™ EA 103 Functional Polymer is produced via a high pressure reactor. It exhibits high flexibility and imparts low temperature toughness to a wide range of engineering resins. It can be ut..
Vicat Softening Point 49.0 °C
120 °F
ASTM D1525, ISO 306
DuPont™ Surlyn® 6320 Magnesium Ionomer
Surlyn® 6320 is a magnesium ionomer thermoplastic resin. It is available for use in conventional extrusion and injection equipment, to create various sheets or shapes. Surlyn® 6320 thermoplastic r..
Vicat Softening Point 49.0 °C
120 °F
ASTM D1525
Arkema Group OREVAC® 9304 EVA Terpolymer
OREVAC® is a range of ethylene-vinyl acetate copolymers modified by adjunction of polar groups which, when molten, have excellent adhesive properties to various substrates. They are supplied as fre..
Vicat Softening Point 49.0 °C

@Load 1.02 kg
120 °F

@Load 2.25 lb
ASTM-D1525
Braskem Evateno® HM 728 EVA Hot Melt Copolymer
Evateno® HM 728 is a copolymer of Ethylene-Vinyl Acetate (EVA) with high vinyl-acetate content, medium molecular weight, and good compatibility with other thermoplastic and elastomeric resins. Evat..
Vicat Softening Point 49.0 °C
120 °F
BASF Novolen® 2700 L Polypropylene
UV stabilized grade for injection molded parts.Data was collected by ISO methods and provided by BASF.
Vicat Softening Point 49.0 °C
120 °F
ASTM D1525
Westlake EMAC® Plus SP1330 22% Ethylene-Methyl Acrylate Copolymer
Westlake EMAC® Plus SP1330 is a 22% EMA copolymer designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal temperatures are required. SP1330 is..
Vicat Softening Point 49.0 °C
120 °F
50°C/h 50N; ISO 306
LATI LATISTAT 48/9900-03 Ethylene Vinyl Acetate (EVA) Base Conductive Plastic  (Unverified Data**)
Description: Latistat materials have low specific resistivity. They feature partial electrical conductivity. Selected functional additives give materials with low specific resistivity and reasonable..
Vicat Softening Point 49.0 °C
120 °F
ASTM D1525
DuPont Appeel® LSR 1181 Modified EVA Lidding Sealing Resin
Appeel® 1181 is an extrusion coatable resin designed to be a sealing layer for lidding applications. It provides peelable seals over a broad temperature range to a number of container materials inc..