Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Elvax® 3182 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade
Manufacturer DuPont Packaging and Industrial Polymers
Trade Name Elvax®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Elvax® 3182 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
28 wt% Vinyl Acetate.Elvax® 3182-2 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. Additives: No slip, No antiblock, Non-BHT antioxidant.General Processing Information: Resin melt temperature should be maintained in the range of 160-215°C (320-420°F) to provide a suitable viscosity for coextrusion in either blown film or cast film applications. Selection of a specific melt temperature will depend not only upon machine variables but also upon the substrate type. Excessively high melt temperatures, above 230°C (446°F) may cause thermal degradation of the resin.Information provided by DuPont Packaging Polymers.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ASTM D792
Melt Flow 3.0 g/10 min
3.0 g/10 min
Condition not noted.; ASTM D1238
Thermal Properties Metric English Comments
Melting Point 51.0 °C
124 °F
Freezing Point via DSC/ASTM D3418
73.0 °C
163 °F
Upon Melting via DSC/ASTM D3418
Vicat Softening Point 49.0 °C
120 °F
ASTM D1525