Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ICO Polymers ICOTEXâ„¢ 520-5076 500 Micron EVA Powder

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate; Molded/Extruded
Manufacturer ICO Polymers (A Schulman Inc.)
Trade Name ICOTEX™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ICO Polymers ICOTEXâ„¢ 520-5076 500 Micron EVA Powder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: ICOTEX 520-5076 is an EVA powder that has been developed to meet the special requirements of the textile coating industry. Its key characteristics are a good melt flow and flexibility, and a vinyl acetate content of 20%. Key Characteristics: high toughness, good melt and strength. Information provided by ICO Polymers.A Schulman acquired ICO, Inc. in 2010.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D1505
Particle Size >= 150 µm
>= 150 µm
pan, 7%
<= 500 µm
<= 500 µm
sieve < 5%
Vinyl Acetate Content 20 %
20 %
wt %; Exxon Mobil
Melt Index of Compound 20 g/10 min

@Load 2.16 kg,
Temperature 190 °C
20 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 6.00 MPa
870 psi
ASTM D638
Elongation at Break 240 %
240 %
50 mm/min; ASTM D638
Thermal Properties Metric English Comments
Melting Point 83.0 °C
181 °F
DSC; ASTM D3418
90.0 °C
194 °F
fusing temperature
Vicat Softening Point 49.0 °C
120 °F
ASTM D1525
Descriptive Properties Value Comments
Max Dry Flow max 37 sec/100g
ASTM