Polymer Property : Flexural Strength = 11600 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 80.0 MPa

@Temperature 23.0 °C
11600 psi

@Temperature 73.4 °F
ASTM D790
DuPont Performance Polymers Crastin® 6130 NC010 PBT  (Unverified Data**)
Crastin® 6130 NC010 is an unreinforced, medium high viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by DuPont Performance Polymers
Flexural Strength 80.0 MPa

@Temperature 125 °C
11600 psi

@Temperature 257 °F
Result based on 450G; ISO 178
Victrex® PEEK 600G Polyetheretherketone  (discontinued **)
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta..
Flexural Strength 80.0 MPa

@Temperature 175 °C
11600 psi

@Temperature 347 °F
ISO 178
Victrex® PEEK 450FC30 General Purpose
Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and ext..
Flexural Strength 80.0 MPa

@Temperature 175 °C
11600 psi

@Temperature 347 °F
ISO 178
Victrex® PEEK 450GL30 30% Glass Fiber Reinforced
Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, F..
Flexural Strength 80.0 MPa

@Temperature 175 °C
11600 psi

@Temperature 347 °F
Result based on 450GL30; ISO 178
Victrex® PEEK 450GL30 Polyetheretherketone, 30% Glass Fiber, Black
Product Description: High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, Standard viscos..
Flexural Strength 80.0 MPa

@Temperature 23.0 °C
11600 psi

@Temperature 73.4 °F
DAM; ISO 178
DuPont Performance Polymers Zytel® 157HSL BK010 Nylon 612  (Unverified Data**)
Zytel® 157HSL BK010 is a heat stabilized, weatherable, lubricated polyamide 612 resin that is suitable for molding and extrusion applications.Information provided by DuPont Performance Polymers
Flexural Strength 80.0 MPa

@Strain 7.00 %
11600 psi

@Strain 7.00 %
cond., 2 mm/min; ISO 178-A
Lanxess Durethan® BKV 215 000000 Nylon 6-Copolymer, Glass Fiber Reinforced, Impact Modified
PA 6-Copolymer, 15% glass fibers, injection molding impact modifiedInformation provided by LANXESS.
Flexural Strength 80.0 MPa

@Temperature 23.0 °C
11600 psi

@Temperature 73.4 °F
Practical Use (Water Absorption 3.0%); ASTM-D790
Toyobo GLAMIDE® T-400G15 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 80.0 MPa

@Temperature 80.0 °C
11600 psi

@Temperature 176 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-422-02 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 80.0 MPa

@Temperature 80.0 °C
11600 psi

@Temperature 176 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® TY-502NZ 6T-Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 80.0 MPa

@Temperature 80.0 °C
11600 psi

@Temperature 176 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® TY-835TC Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 80.0 MPa

@Treatment Temp. 150 °C,
Time 3600 sec
11600 psi

@Treatment Temp. 302 °F,
Time 1.00 hour
ISO 178; IEC/EN 60893-2 5.1
Elektro-Isola G-Etronax PM GPO 3 Polyester, Glass Mat, Red, Sheets
Description: Good electrical properties such as high breakdown voltage in air and oil and highest arc resistance and tracking resistance. Self-extinguishing. Low smoke emission, halogen-free.Applica..
Flexural Strength 80.0 MPa

@Strain 3.50 %,
Temperature 23.0 °C
11600 psi

@Strain 3.50 %,
Temperature 73.4 °F
ISO 178
DuPont Performance Polymers Delrin® 111P NC010 Acetal Homopolymer
Delrin® 111P is a high viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, fewer voids). It has higher tensile strength and mod..
Flexural Strength 80.0 MPa

@Temperature 175 °C
11600 psi

@Temperature 347 °F
ISO 178
Victrex® PEEK 150FC30 Easy Flow
Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy ..