Mechanical Properties Metric English Comments
Tear Strength 16.0 kN/m
91.3 pli
ISO 34-1
PolyOne OnFlex™ S KG 40A-3S2016 Thermoplastic Elastomer (TPE)
OnFlex™-S KG thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to polyamide p..
Tear Strength 16.0 kN/m
91.3 pli
Die B
Momentive Performance Materials TSE 221-8U Heat Cured Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Tear Strength 16.0 kN/m
91.3 pli
Die B
Momentive Performance Materials Electro 170 Heat Cured Rubber - High Voltage Insulating
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Tear Strength 16.0 kN/m
91.3 pli
ISO 6383
SABIC Innovative Plastics NORYL WCP761 PPE-TPE
Flexible Noryl injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in overmolding applications such as plugs, strain re..
Tear Strength 16.0 kN/m
91.0 pli
Die B; DCBP Cure
Shin-Etsu Silicones KE-551U Silicone Rubber
KE551U is one of a series of easy processing, general purpose grade silicone rubber bases. It can be used in a variety of applications requiring finishing by molding or extruding with extending fill..
Tear Strength 16.0 kN/m
91.3 pli
Die C; Cross direction; ASTM D624
Teknor Apex Sarlink® 3440 Thermoplastic Elastomer
A NSF certified, low hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inject..
Tear Strength 16.0 kN/m
91.0 pli
Notched, Die B; ASTM D 624
CPT C-Flex® R70-081 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Tear Strength 16.0 kN/m
91.4 pli
Dow Corning 3631 PART A&B KIT
Two-part, solvent free, heat-cured liquid silicone rubber.Information provided by Dow Corning
Tear Strength 16.0 kN/m
91.3 pli
ACC MM911 Condensation Cure 2-Part Molding Rubber
Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: high tear strength, picks up extremely fine details, low viscosity, good resistance to styrene attack, easy degassing..
Tear Strength 16.0 kN/m
91.3 pli
ISO 34-B
AlphaGary Evoprene™ 3276 Standard SBS Thermoplastic Elastomer Compound
Tear Strength 16.0 kN/m
91.3 pli
Trelleborg Commercial Neoprene® C803 Chloroprene
CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grade..
Tear Strength 16.0 kN/m
91.0 pli
Die B, Silicone Property; ASTM D624
Arlon R37732R079 0.079" (2.01 mm) Cured Silicone Rubber with FEP Film Substrate
Design/Construction: Interleave: PolyethyleneSide 1: Cured Silicone RubberSubstrate: FEP FilmAppearance: Red silicone rubber chemically bonded to fluoropolymer filmThis data represents typical value..
Tear Strength 16.0 kN/m
91.3 pli
angle
Momentive Performance Materials XE23-703U Heat Cured Rubber - Electro Conductive
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..