Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Teknor Apex Uniprene® 55A Polyvinyl Chloride, Flexible

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade
Manufacturer Teknor Apex Company
Trade Name UNIPRENE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Uniprene® 55A Polyvinyl Chloride, Flexible.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: High Elastic RecoveryInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
5 seconds; ASTM D2240
Tensile Strength at Break 3.86 MPa
560 psi
ASTM D412
Elongation at Break 300 %
300 %
ASTM D412
100% Modulus 0.00214 GPa
0.310 ksi
ASTM D412
Tear Strength 16.0 kN/m
91.3 pli
Die C; ASTM D624
Compression Set 20 %

@Temperature -5.00 °C,
Time 79200 sec
20 %

@Temperature 23.0 °F,
Time 22.0 hour
Method B; ASTM D395
27 %

@Temperature 21.1 °C,
Time 79200 sec
27 %

@Temperature 70.0 °F,
Time 22.0 hour
Method B; ASTM D395
35 %

@Temperature 37.8 °C,
Time 79200 sec
35 %

@Temperature 100 °F,
Time 22.0 hour
Method B; ASTM D395
Copyright © lookpolymers.com All Rights Reserved