Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tear Strength = 91.3 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 16.0 kN/m
91.3 pli
ISO 34-1
PolyOne OnFlex™ S KG 40A-3S2016 Thermoplastic Elastomer (TPE)
OnFlex™-S KG thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to polyamide p..
Tear Strength 16.0 kN/m
91.3 pli
Die B
Momentive Performance Materials FSE7520 Heat Cured Fluorosilicone Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Tear Strength 16.0 kN/m
91.3 pli
Die B
Momentive Performance Materials Siloprenâ„¢ Electro 242-1 Electrically Insulating Liquid Silicone Rubber
This LSR elastomer is an electrically insulating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate..
Tear Strength 16.0 kN/m
91.3 pli
Die B
Momentive Performance Materials TSE 221-8U Heat Cured Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Tear Strength 16.0 kN/m
91.3 pli
Die B
Momentive Performance Materials Electro 170 Heat Cured Rubber - High Voltage Insulating
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Tear Strength 16.0 kN/m
91.3 pli
Die C; Cross direction; ASTM D624
Teknor Apex Sarlink® 3135 Thermoplastic Elastomer
A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3135 can be processed by injection molding or extrusion for ap..
Tear Strength 16.0 kN/m
91.3 pli
ASTM D624
ELASTO UK Dryflex® 500300S SEBS Based Material, Unfilled Qualities, 30A Hardness, Translucent
The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha..
Tear Strength 16.0 kN/m
91.3 pli
ACC MM911 Condensation Cure 2-Part Molding Rubber
Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: high tear strength, picks up extremely fine details, low viscosity, good resistance to styrene attack, easy degassing..
Tear Strength 16.0 - 37.0 kN/m
91.3 - 211 pli
ASTM D 624
API Megol AM DP2339 SEBS Adhesion Modified Overmolding for PA
Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as ..
Tear Strength 16.0 kN/m
91.3 pli
ASTM D 624
API Megol AM DP2375/30 SEBS Adhesion Modified Overmolding for Polar Polymers
Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as ..
Tear Strength 16.0 kN/m
91.3 pli
ISO 34-B
AlphaGary Evoprene™ 3276 Standard SBS Thermoplastic Elastomer Compound
Tear Strength 16.0 kN/m
91.3 pli
angle
Momentive Performance Materials XE23-703U Heat Cured Rubber - Electro Conductive
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Copyright © lookpolymers.com All Rights Reserved