Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon 22122R079 0.079" Cured Silicone Rubber and FEP Film Laminate

Category Polymer , Thermoplastic , Fluoropolymer , FEP , Thermoset , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 22122R079 0.079" Cured Silicone Rubber and FEP Film Laminate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction:Interleave: 3 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: 0.005" FEP FilmThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 127 microns
5.00 mil
Substrate; Arlon SQA-TMS-003
1880 microns
74.0 mil
Side 1; Arlon SQA-TMS-003
2010 microns
79.0 mil
Overall Thickness; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 65
65
Silicone Property; ASTM D2240
Tensile Strength 7.433 MPa
1078 psi
Silicone Property; ASTM D412
Elongation at Break 341 %
341 %
Silicone Property; ASTM D412
Tear Strength 16.0 kN/m
91.0 pli
Die B, Silicone Property; ASTM D624
Peel Strength 2.07 kN/m
11.8 pli
Silicone to FEP Bond Strength
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Electrical Properties Metric English Comments
Dielectric Strength >= 19.1 kV/mm
>= 486 kV/in
ASTM D149
Processing Properties Metric English Comments
Shelf Life 60.0 Month

@Temperature 21.1 °C
60.0 Month

@Temperature 70.0 °F
Descriptive Properties Value Comments
Color Red
Transparent
Substrate
Total Product Weight (oz/yd2) 77
Arlon SQA-TMS-025