Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon R37732W079 0.079" (2.01 mm) Cured Silicone Rubber with Treated FEP Film Substrate

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon R37732W079 0.079" (2.01 mm) Cured Silicone Rubber with Treated FEP Film Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction: Interleave: PolyethyleneSide 1: Cured Silicone RubberSubstrate: Treated FEP FilmThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 76.2 microns
3.00 mil
Interleave
127 microns
5.00 mil
Substrate
1880 microns
74.0 mil
Side 1; Arlon SQA-TMS-003
2010 microns
79.0 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 65
65
Silicone Property; ASTM D2240
Tensile Strength 7.433 MPa
1078 psi
Silicone Property; ASTM D412
Elongation at Break 341 %
341 %
Silicone Property; ASTM D412
Tear Strength 16.0 kN/m
91.0 pli
Die B, Silicone Property; ASTM D624
Peel Strength 2.07 kN/m
11.8 pli
Silicone to FEP Bond Strength; Arlon SQA-TMS-011
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 19.1 kV/mm
486 kV/in
ASTM D149
Processing Properties Metric English Comments
Shelf Life 60.0 Month

@Temperature 21.1 °C
60.0 Month

@Temperature 70.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Transparent
Substrate
White
Total Product Weight (oz/yd2) 77