Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 16.0 kN/m | 91.0 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Santoprene® 281-55MED Thermoplastic Elastomer
(discontinued **) A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of our medical grad.. |
|||
Tear Strength | 16.0 kN/m | 91.0 pli | 73°F; ASTM D624 |
Advanced Elastomer Systems Santoprene® 8281-45W237 Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other .. |
|||
Tear Strength | 16.0 kN/m | 91.0 pli | ASTM D624 |
STAR Thermoplastic Alloys & Rubbers StarMediflex P 7050-1000 TPE Product Description: StarMediflex P 7050-1000 is an easy processing TPE designed for injection molding. This particular class of TPE material for medical products and tubing applications. Features:S.. |
|||
Tear Strength | 16.0 kN/m | 91.0 pli | Die B; DCBP Cure |
Shin-Etsu Silicones KE-551U Silicone Rubber KE551U is one of a series of easy processing, general purpose grade silicone rubber bases. It can be used in a variety of applications requiring finishing by molding or extruding with extending fill.. |
|||
Tear Strength | 16.0 kN/m | 91.0 pli | |
Dow Corning HV 1760/80 SILICONE RUBBER NATURAL 80 Shore hardness high consistency silicone rubber with fast cure system and excellent tracking and erosion resistanceInformation provided by Dow Corning |
|||
Tear Strength | 16.0 kN/m | 91.0 pli | Notched, Die B; ASTM D 624 |
CPT C-Flex® R70-081 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Tear Strength | 16.0 kN/m | 91.0 pli | Die B, Silicone Property; ASTM D624 |
Arlon 22122R079 0.079" Cured Silicone Rubber and FEP Film Laminate Design/Construction:Interleave: 3 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: 0.005" FEP FilmThis data represents typical values for the production material and should not be used as .. |
|||
Tear Strength | 16.0 kN/m | 91.0 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Santoprene® 171-55 Thermoplastic Elastomer
(discontinued **) A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as those.. |
|||
Tear Strength | 16.0 kN/m | 91.0 pli | Die B, Silicone Property; ASTM D624 |
Arlon R37732R079 0.079" (2.01 mm) Cured Silicone Rubber with FEP Film Substrate Design/Construction: Interleave: PolyethyleneSide 1: Cured Silicone RubberSubstrate: FEP FilmAppearance: Red silicone rubber chemically bonded to fluoropolymer filmThis data represents typical value.. |
|||
Tear Strength | 16.0 kN/m | 91.0 pli | Die B, Silicone Property; ASTM D624 |
Arlon R37732W079 0.079" (2.01 mm) Cured Silicone Rubber with Treated FEP Film Substrate Design/Construction: Interleave: PolyethyleneSide 1: Cured Silicone RubberSubstrate: Treated FEP FilmThis data represents typical values for the production material. The data should not be used to w.. |