Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 16.0 kN/m | 91.4 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Santoprene® 201-55 Thermoplastic Elastomer A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Tear Strength | 16.0 kN/m | 91.4 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Santoprene® 271-55 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Tear Strength | 16.0 kN/m | 91.4 pli | 73°C, Die C, Across Flow; ASTM D624 |
ExxonMobil Santoprene® 101-55 Thermoplastic Elastomer A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Tear Strength | 16.0 kN/m | 91.4 pli | |
Dow Corning 3631 PART A&B KIT Two-part, solvent free, heat-cured liquid silicone rubber.Information provided by Dow Corning |