Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.05 - 12.4 GPa | 153 - 1800 ksi | Average value: 9.87 GPa Grade Count:16 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Flexural Modulus | 2.40 - 12.4 GPa | 348 - 1800 ksi | Average value: 4.96 GPa Grade Count:115 |
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a.. |
|||
Flexural Modulus | 0.0260 - 12.4 GPa | 3.77 - 1800 ksi | Average value: 1.44 GPa Grade Count:725 |
Overview of materials for Polypropylene, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Flexural Modulus | 0.255 - 12.4 GPa | 37.0 - 1800 ksi | Average value: 2.85 GPa Grade Count:99 |
Overview of materials for Nylon 66, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum .. |
|||
Flexural Modulus | 3.70 - 12.4 GPa | 537 - 1800 ksi | Average value: 7.80 GPa Grade Count:122 |
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma.. |
|||
Flexural Modulus | 4.48 - 12.4 GPa | 650 - 1800 ksi | Average value: 7.74 GPa Grade Count:10 |
Overview of materials for Nylon 66, Mineral Filled, NCG Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, NCG Fiber Filled". Each property range of values reported is minimum and maxim.. |
|||
Flexural Modulus | 11.0 - 12.4 GPa | 1600 - 1800 ksi | ASTM D790 |
Mar-Bal MB1000-15 Thermoset Polyester Composite Molding Compound A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro.. |
|||
Flexural Modulus | 10.3 - 12.4 GPa | 1500 - 1800 ksi | ASTM D790 |
Mar-Bal MB2000-15 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |
|||
Flexural Modulus | 11.0 - 12.4 GPa | 1600 - 1800 ksi | ASTM D790 |
Mar-Bal MB5500 Thermoset Polyester Composite Molding Compound A superior heat resistant material. U.L. RTI rating of 160°C-170°C.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc. |
|||
Flexural Modulus | 11.0 - 12.4 GPa | 1600 - 1800 ksi | |
Bulk Molding Compounds BMC 350 Thermoset Polyester, Medium Impact BMC 350 is a cosmetic and appliance grade material with excellent heat and stain resistant properties. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk.Typical ap.. |
|||
Flexural Modulus | 11.0 - 12.4 GPa | 1600 - 1800 ksi | |
Bulk Molding Compounds BMC 850 Corrosion Resistant, Flame Retardant Molding Compound BMC 850 is a high strength, corrosion resistant and flame retardant molding compound. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk form.Typical applications a.. |
|||
Flexural Modulus | 10.3 - 12.4 GPa | 1500 - 1800 ksi | |
Bulk Molding Compounds BMC 902 Thermoset Polyester, Soft Flow Encapsulation Grade BMC 902 is a medium strength, high flow molding compound that meets Ford Specification ESFM3D114- A. BMC 902 has excellent electrical properties and creep resistance. It can be pigmented in a wide r.. |
|||
Flexural Modulus | 11.7 - 12.4 GPa | 1700 - 1800 ksi | |
Bulk Molding Compounds BMC T15(GP) General Purpose Molding Compound BMC T15(GP) is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15(GP) is well suited for a variety of applications. It is av.. |
|||
Flexural Modulus | 11.0 - 12.4 GPa | 1600 - 1800 ksi | |
Bulk Molding Compounds BMC 851 Corrosion Resistant, Flame Retardant Molding Compound BMC 851is a high strength, corrosion resistant and flame retardant molding compound. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk form.Typical applications ar.. |
|||
Flexural Modulus | 10.3 - 12.4 GPa | 1500 - 1800 ksi | |
Bulk Molding Compounds BMC 900 Thermoset Polyester, Soft Flow Encapsulation Grade BMC 900 is an encapsulation grade, soft flow material. As with all other BMCI compounds, this series can be supplied in logs, slugs or bulk.Typical applications are electrical coil encapsulations an.. |
|||
Flexural Modulus | 3.45 - 12.4 GPa | 500 - 1800 ksi | Average value: 8.27 GPa Grade Count:4 |
Overview of materials for Acrylic, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values o.. |
|||
Flexural Modulus | 9.70 - 12.4 GPa | 1410 - 1800 ksi | ASTM D790-70 |
Budd DSM-949, Diesel Grade SMC, Vinyl Ester, Black
(discontinued **) Used for parts requiring high strength at room temperature, good retention of properties at high temperatures and corrosion resistance, such as diesel engine external body parts.Data provided by the.. |