Material Notes:
General purpose SANGood chemical resistance, excellent dimensional stabilityInformation provided by Cossa Polimeri S.r.l.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D 792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D 955
Melt Flow 25 g/10 min

@Load 10.0 kg,
Temperature 220 °C
25 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 70.0 MPa
10200 psi
ASTM D 638
Elongation at Break 3.0 %
3.0 %
ASTM D 638
Flexural Modulus 3.70 GPa
537 ksi
ASTM D 790
Izod Impact, Notched 0.200 J/cm

@Temperature 23.0 °C
0.375 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Thermal Properties Metric English Comments
Vicat Softening Point 102 °C

@Load 5.00 kg
216 °F

@Load 11.0 lb
50°C/hr; ASTM D 1525
108 °C

@Load 0.999 kg
226 °F

@Load 2.20 lb
50°C/hr; ASTM D 1525
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in