Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman ComAlloy Hiloy® 636 Nylon 6/6, Glass/Mineral Reinforced, Flow Enhanced

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass/Mineral Filled
Manufacturer A. Schulman ComAlloy
Trade Name Hiloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman ComAlloy Hiloy® 636 Nylon 6/6, Glass/Mineral Reinforced, Flow Enhanced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, ComAlloy International Company.40% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Density 1.49 g/cc
0.0538 lb/in³
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 119
119
ASTM D785
Tensile Strength, Ultimate 68.0 MPa
9860 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Flexural Strength 99.0 MPa
14400 psi
ASTM D790
Flexural Modulus 4.70 GPa
682 ksi
ASTM D790
Izod Impact, Notched 0.430 J/cm
0.806 ft-lb/in
ASTM D256
Izod Impact, Unnotched 3.63 J/cm
6.80 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 255 - 275 °C
491 - 527 °F
Deflection Temperature at 0.46 MPa (66 psi) 219 °C
426 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 150 °C
302 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 290 °C
554 °F
Approximate middle barrel temperature.
Users viewing this material also viewed the following: