Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay TECHNYL® B 216 V30 Black 3 N PA66, 30% glass fiber, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Solvay
Trade Name Technyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® B 216 V30 Black 3 N PA66, 30% glass fiber, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Copolyamide 66/6, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHNYL® B 216 V30 is used in all sectors of industry, offering an excellent combination between thermal and mechanical properties. This grade is commonly used in the automotive industry, for the production of colored internal parts of car. This product is available in black.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 115 MPa
16700 psi
ISO 527 Type 1A
Tensile Strength, Yield 115 MPa
16700 psi
ISO 527 type 1 A
Elongation at Break 8.0 %
8.0 %
ISO 527 Type 1A
Tensile Modulus 6.50 GPa
943 ksi
ISO 527 Type 1A
Flexural Modulus 4.70 GPa
682 ksi
ISO 178
Izod Impact, Notched (ISO) 19.0 kJ/m²
9.04 ft-lb/in²
ISO 180/1eA
Charpy Impact Unnotched 9.20 J/cm²
43.8 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 1.60 J/cm²
7.61 ft-lb/in²
ISO 179/1eA
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Constant 4.0
4.0
IEC 60250
Dielectric Strength 26.0 kV/mm
660 kV/in
IEC 60243
Dissipation Factor 0.10
0.10
IEC 60250
Comparative Tracking Index 475 V
475 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %