Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.63 GPa | 381 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Packaging 2160 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Modulus | 2.63 GPa | 381 ksi | Tangent; ISO 178 |
Mytex Polymers AS33K(W)-02 Polypropylene, Talc filled, Compounded Description: Talc filled compounded polypropylene produced for automotive interior applications using Mytex® Technology.Key Applications: General purpose interiorInformation provided by Mytex Polym.. |
|||
Flexural Modulus | 2.63 GPa | 381 ksi | ASTM D790 |
Network Polymers Kepital® F30-03 Description: Natural Acetal CopolymerInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 2.63 GPa | 381 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® CY2010 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
Flexural Modulus | 2.63 GPa | 381 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® CY5000 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
Flexural Modulus | 2.63 GPa | 381 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® CY5000 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
Flexural Modulus | 2.63 GPa | 381 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Cycoloy® CY5000 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
Flexural Modulus | 2.63 GPa | 381 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® CY5005 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
Flexural Modulus | 2.63 GPa | 381 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Cycoloy® CY5005 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
Flexural Modulus | 2.63 GPa | 381 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Cycoloy® CY6010 PC+ABS Cycoloy CY6010 resin is a flame retardant PC/ABS blend featuring excellent flow together with good impact and UL-94 V0 listing at 1.5mm. Its excellent flow combined with balanced heat and good pract.. |
|||
Flexural Modulus | 2.63 GPa | 381 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Cycoloy® CY6010 PC+ABS (Asia Pacific) Cycoloy CY6010 resin is a flame retardant PC/ABS blend featuring excellent flow together with good impact and UL-94 V0 listing at 1.5mm. Its excellent flow combined with balanced heat and good pract.. |
|||
Flexural Modulus | 2.63 GPa | 381 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Cycoloy® CY6010 PC+ABS (Europe-Africa-Middle East) Cycoloy CY6010 resin is a flame retardant PC/ABS blend featuring excellent flow together with good impact and UL-94 V0 listing at 1.5mm. Its excellent flow combined with balanced heat and good pract.. |
|||
Flexural Modulus | 2.63 GPa | 381 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® DMX1214 PC Copolymer (Asia Pacific) This product will be phased out per January 2015 -- Lexan* DMX1214 resin is an improved flow, transparent copolycarbonate resin with improved scratch resistance. |
|||
Flexural Modulus | 2.63 GPa | 381 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® DMX1214 PC Copolymer (Europe-Africa-Middle East) This product will be phased out per January 2015 -- Lexan* DMX1214 resin is an improved flow, transparent copolycarbonate resin with improved scratch resistance. |
|||
Flexural Modulus | 2.63 GPa | 381 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® ML7677 PC (Asia Pacific) Transparent Polycarbonate in limited colors. Excellent processability, super high flow, flame retardant, UL rated V-1 at 2.0mm |
|||
Flexural Modulus | 2.63 GPa | 381 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® DMX1214 PC Copolymer Lexan* DMX1214 resin is an improved flow, transparent copolycarbonate resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.63 GPa | 381 ksi | ASTM D790 |
Asahi Kasei Tenac®-C 7510 Acetal Copolymer, High Flow
(discontinued **) High-flow grade, suited for thin-wall, long-flow-distance moldings.Applications: Lighters, aerosol bottles, fasteners.This product is not a part of the standard product line dated 2003. |
|||
Flexural Modulus | 2.63 GPa | 381 ksi | ASTM D790 |
Asahi Kasei Tenac®-C 8554 Acetal Copolymer, High Flow
(discontinued **) Superhigh-flow grade, with properties necessary for VCR reels.Applications: VCR reels.This product is not a part of the standard product line dated 2003. |
|||
Flexural Modulus | 2.63 GPa | 381 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP IAL12 PA6.12 LNP* LUBRICOMP* IAL12 is a compound based on Nylon 6/12 resin containing 5% PTFE, 10% Aramid Fiber. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 2.63 GPa | 381 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Lubricomp KI001A Acetal LNP* Lubricomp Fulton 441D is an Acetal based compound with Silicone.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.63 GPa | 381 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP EP003 PEI LNP* Lubricomp EP003 is a Polyetherimide containing 15% PTFE/Silicone. Added features include: Internally Lubricated. |
|||
Flexural Modulus | 2.63 GPa | 381 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON FX98501 PE (Asia Pacific) LNP* Stat-kon* FX98501 is a compound based on Polyethylene resin containing Glass Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 2.63 GPa | 381 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL EXNL0357 PPE+PS |
|||
Flexural Modulus | 2.63 GPa | 381 ksi | ISO 178 |
Polyplastics Duranex® 2002 Polybutylene Terephthalate (PBT), Standard DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Modulus | 2.63 GPa | 381 ksi | ISO 178 |
Polyplastics Duranex® 2002U Polybutylene Terephthalate (PBT), Weather resistance DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Modulus | 2.63 GPa | 381 ksi | 2mm/min; ISO 178 |
Borealis ME212U Polypropylene Compound, Mineral Filled ME212U is a 20% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: air ducts, air.. |
|||
Flexural Modulus | 2.63 GPa | 381 ksi | ASTM D790 |
ABW Polymers PC/PET Alloy Typical property data below. Material may be tailored to meet specific requirements. This data should be used only as a guide and no assurance can be granted by the company that all molded articles.. |
|||
Flexural Modulus | 2.63 GPa | 381 ksi | ASTM D790 |
Solvay Specialty Polymers Mindel® S-1000 Modified Polysulfone
(discontinued **) This product line was acquired by Solvay Advanced Polymers from BP Amoco in November 2001. |