Material Notes:
Typical property data below. Material may be tailored to meet specific requirements. This data should be used only as a guide and no assurance can be granted by the company that all molded articles will exhibit duplicate properties as those listed.Information provided by ABW Polymers.
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
ASTM D792
Melt Flow 19.1 g/10 min

@Load 5.00 kg,
Temperature 265 °C
19.1 g/10 min

@Load 11.0 lb,
Temperature 509 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 62.1 MPa
9010 psi
ASTM D638
Elongation at Break 130 %
130 %
ASTM D638
Flexural Modulus 2.63 GPa
381 ksi
ASTM D790
Izod Impact, Notched 6.90 J/cm
12.9 ft-lb/in
ASTM D256
4.30 J/cm

@Temperature -40.0 °C
8.06 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 255 °C
491 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 222 °C
432 °F
ASTM D648
Flammability, UL94 V-2
V-2
Pending