Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Styron Magnumâ„¢ 1250 BG Acrylonitrile Butadiene Styrene (ABS)

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer Styron
Trade Name Magnum™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron Magnumâ„¢ 1250 BG Acrylonitrile Butadiene Styrene (ABS).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High Impact, High Heat, Blow Molding ABSInformation provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Physical Properties Metric English Comments
Density 1.046 g/cc
0.03779 lb/in³
ASTM D792B
Melt Flow 1.7 g/10 min

@Load 3.80 kg,
Temperature 230 °C
1.7 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 33.6 MPa
4870 psi
ASTM D638
Elongation at Break 60 %
60 %
ASTM D638
Flexural Modulus 2.01 GPa
292 ksi
ASTM D790A
Izod Impact, Notched 3.58 J/cm
6.70 ft-lb/in
ASTM D256A
1.87 J/cm

@Temperature -30.0 °C
3.50 ft-lb/in

@Temperature -22.0 °F
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 103 °C
217 °F
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 86.7 °C
188 °F
unannealed; ASTM D648
Users viewing this material also viewed the following: