Material Notes:
Applications:extrusion sheetrefrigerator door liners and inner box linerspicnic coolerssnow boatsluggage cases
Physical Properties Metric English Comments
Melt Flow 7.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
7.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105

@Thickness 6.35 mm,
Temperature 23.0 °C
105

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D785
Tensile Strength, Ultimate 43.1 MPa

@Temperature 23.0 °C
6260 psi

@Temperature 73.4 °F
ASTM D638
Flexural Yield Strength 59.3 MPa

@Temperature 23.0 °C
8610 psi

@Temperature 73.4 °F
ASTM D790
Flexural Modulus 2.01 GPa

@Temperature 23.0 °C
292 ksi

@Temperature 73.4 °F
ASTM D790
Izod Impact, Notched 2.94 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
5.51 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 92.0 °C

@Thickness 6.35 mm
198 °F

@Thickness 0.250 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C

@Thickness 6.35 mm
185 °F

@Thickness 0.250 in
ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
HB

@Thickness 3.12 mm
HB

@Thickness 0.123 in
Processing Properties Metric English Comments
Processing Temperature 180 - 240 °C
356 - 464 °F
Drying Temperature 80.0 - 90.0 °C

@Time 7200 - 18000 sec
176 - 194 °F

@Time 2.00 - 5.00 hour