Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shinkong Synthetic Fibers Shinblend® A724 PC/PBT, High Impact

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shinkong Synthetic Fibers Shinblend® A724 PC/PBT, High Impact.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information from Shinkong Synthetic Fibers Corp.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Water Absorption 0.14 %
0.14 %
ASTM D570
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 53.9 MPa
7820 psi
ASTM D638
Elongation at Break 10 %
10 %
ASTM D638
Flexural Yield Strength 75.5 MPa
11000 psi
ASTM D790
Flexural Modulus 2.01 GPa
292 ksi
ASTM D790
Izod Impact, Notched 7.35 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
13.8 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
7.85 J/cm

@Thickness 3.17 mm,
Temperature -20.0 °C
14.7 ft-lb/in

@Thickness 0.125 in,
Temperature -4.00 °F
ASTM D256
8.83 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
16.5 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 105 °C
221 °F
ASTM D648
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved