Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CPC - Vycom FLAMETEC™ HALAR® 901 Opaque Ethylene Chlorotrifluoroethylene (ECTFE)

Category Polymer , Thermoplastic , Fluoropolymer , ETFE/ECTFE
Manufacturer CPC - Vycom Co.
Trade Name FLAMETEC™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CPC - Vycom FLAMETEC™ HALAR® 901 Opaque Ethylene Chlorotrifluoroethylene (ECTFE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flametec™ Halar® ECTFE (Ethylene Chlorotrifluoroethylene) is an ultra-pure fluoropolymer that is a tough engineering thermoplastic with a balance of physical and chemical properties that qualify it for high performance service in a wide range of applications. It is mechanically both strong and tough, exhibiting high dielectric strength, and can be used in applications over a broad temperature range. As a fluoropolymer, it is highly resistant to most environmental conditions, including corrosive chemicals and organic solvents, strong acids, alkaline, peroxide and SC1 and SC2 chemistries, and aqueous caustics for handling wet or dry chlorine, bromine, and other halogens.FEATURES AND BENEFITS Purity- Halar has a very low extractable and leaching levels for the most demanding semiconductor applications. Weldability- Easy to fabricate with conventional welding equipment. Extremely strong welds. Strength- High tensile properties and it is very ductile. Economics- The cost of Halar is easily offset by the expense that would normally be incurred by fire suppression equipment. Fire Safe- Accepted in accordance to FM4910, fire safe materials for clean room construction. Extruded Sheet- Offers the best gauge consistency, surface and tolerances.Information provided by Compression Polymers Corp - Vycom
Physical Properties Metric English Comments
Density 1.68 g/cc
0.0607 lb/in³
ASTM D792
Water Absorption <= 0.10 %
<= 0.10 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ASTM D785
Hardness, Shore D 71
71
ASTM D785
Tensile Strength, Ultimate 53.8 MPa
7800 psi
ASTM D638
Tensile Strength, Yield 29.6 MPa
4300 psi
ASTM D638
Elongation at Break 250 %
250 %
ASTM D638
Flexural Modulus 1.69 GPa
245 ksi
ASTM D790
Izod Impact, Notched NB
NB
ASTM D256
1.23 J/cm

@Temperature -40.0 °C
2.30 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Taber Abrasion, mg/1000 Cycles 0.0060
0.0060
ASTM D1044
Thermal Properties Metric English Comments
CTE, linear 101 µm/m-°C

@Temperature 20.0 °C
56.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Maximum Service Temperature, Air 149 °C
300 °F
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
ASTM D648
Oxygen Index >= 52 %
>= 52 %
ASTM D863
Descriptive Properties Value Comments
Biofilm Buildup 1
CDI
Factory Mutual 4910 Listed
File #4D7Q9.AM
Mean Roughness 0.15
SDI
Notch Sensitivity Not Sensitive