Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ineos H07B-00 Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos H07B-00 Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This is a polypropylene homopolymer for cast film applications that require antiblock additives. This resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.ApplicationsCast filmFlexible packagingBenefitsAntiblock additivesProcessabilityInformation provided by Ineos Olefins & Polymers USA
Physical Properties Metric English Comments
Melt Flow 7.3 g/10 min

@Load 2.16 kg,
Temperature 230 °C
7.3 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 37.40 MPa

@Temperature 23.0 °C
5425 psi

@Temperature 73.4 °F
ASTM D638
Flexural Modulus 1.69 GPa

@Temperature 23.0 °C
245 ksi

@Temperature 73.4 °F
ASTM D790A
Izod Impact, Notched 0.374 J/cm

@Temperature 23.0 °C
0.700 ft-lb/in

@Temperature 73.4 °F
1/8'' notched bar; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 97.8 °C
208 °F
ASTM D648
Users viewing this material also viewed the following: