Mechanical Properties Metric English Comments
Flexural Modulus 1.76 GPa
255 ksi
Tangent; ASTM D790
RheTech Products T10UP100-01 10% Talc Reinforced Polypropylene Copolymer, General Purpose Black, UL94 HB Rated
Applications: Wire troughElectrical componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 1.76 GPa
255 ksi
ASTM D790
Omni Plastics OmniTuff™ CPP CCF30 Copolymer Polypropylene Calcium Carbonate Filled
Applications: Structural parts across industry segments including pump housings, wheels, handles, mountings, brackets, levers, pressure vessels, and furniture components.Information provided by Omni..
Flexural Modulus 1.76 GPa
255 ksi
ASTM D790
Polymer Resources PPX-GP4 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 210F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
Flexural Modulus 1.76 GPa
255 ksi
ASTM D790
Polymer Resources PPX-GP4-IM Modified-PPO, Impact Modified
Modified-Polyphenylene Oxide, Impact Modified, 210F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
Flexural Modulus 1.76 GPa
255 ksi
ASTM D790
Ravago Manufacturing Americas Hylon® N1200STHL BK Nylon 6/6
Available in North America Additive: Heat Stabilizer and Lubricant Features: Lubricated, Good Toughness and Heat StabilizedRoHS CompliantForm: Pellets Color: BlackInformation provided by Ravago.
Flexural Modulus 1.76 GPa
255 ksi
0.05 in/min; 1% secant; Procedure A; ASTM D790
Phillips 66 COPYLENE® CH120LN Polypropylene, Homopolymer, Injection Molding, Antistat/Lube
COPYLENE™ CH120LN is designed for general purpose injection molding applications with anti-static and nucleation. Applications: Food Containers, Housewares, Closures.Information provided by Phillip..
Flexural Modulus 1.76 GPa
255 ksi
0.05 in/min; 1% secant; Procedure A; ASTM D790
Phillips 66 COPYLENE® CH350LN Polypropylene, Homopolymer, High Flow, Nucleated, Lube, Injection Molding
COPYLENE™ CH350LN is designed for general purpose injection molding applications with anti-static, nucleation and controlled rheology. Applications: Food Containers, Housewares, Closures.Informatio..
Flexural Modulus 1.76 - 2.80 GPa
255 - 406 ksi
Average value: 2.26 GPa Grade Count:56
Overview of materials for Polyphenylene Ether, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap..
Flexural Modulus 1.76 - 3.40 GPa
255 - 493 ksi
Average value: 2.41 GPa Grade Count:8
Overview of materials for Polyphenylene Ether, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Impact Grade". Each property range of values reported is minimum and maximum values..
Flexural Modulus 1.76 GPa
255 ksi
ASTM D790
Polymer Resources PPX-GP4 Modified PPO, General Purpose with HDT of 210 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Flexural Modulus 1.76 GPa
255 ksi
0.05 in/min; 1% secant; Procedure A; ASTM D790
Phillips 66 COPYLENE® CH200LN Polypropylene, Homopolymer, CR, Antistat, Nucleated, Injection Molding
COPYLENE™ CH200LN is designed for general purpose injection molding applications with anti-static, nucleation and controlled rheology. Applications: Food Containers, Housewares, Closures.Informatio..
Flexural Modulus 1.76 - 22.5 GPa
255 - 3260 ksi
Average value: 16.4 GPa Grade Count:9
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl..
Flexural Modulus 1.76 GPa
255 ksi
ASTM D790
M. Holland Company PP710 Polypropylene Homopolymer
AntistaticHomopolymerNarrow molecular wt. dist.NucleatedApplications: CapsClosuresConsumer applications
Flexural Modulus 1.76 GPa
255 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP ML004S PP
LNP* LUBRICOMP* ML004S is a compound based on Polypropylene resin containing 20% PTFE. Added features of this material include: Wear Resistant, Heat Stabilized.
Flexural Modulus 1.76 GPa
255 ksi
ASTM D790
Techmer ES Elastoblend® PA6/6 GF4 IM L LE
Availability: North AmericaForms: PelletsAdditive: Lubricant and Impact ModifierFeatures: Lubricant, Low Extractables and Impact ModifiedAppearance: Natural ColorInformation provided by TP Composite..
Flexural Modulus 1.76 GPa
255 ksi
ASTM D790
Techmer ES Electrablend® PA12 CB
Availability: North AmericaForms: PelletsAdditive: Carbon BlackFeatures: ConductiveAppearance: BlackTPCI# 9874105Information provided by TP Composites, Inc.
Flexural Modulus 1.76 GPa
255 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP STAT-KON RX08408 PA 66
LNP* STAT-KON* RX08404 is a compound based on Nylon 66 containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact.
Flexural Modulus 1.76 GPa
255 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Stat-kon RX08408_NA1D004 PA 66
LNP* Stat-Kon* RX08404_NA1D004 is a compound based on Nylon 66 containing Carbon Powder. Characteristics of this grade include: Electrically Conductive, High Impact.This data was supplied by SABI..
Flexural Modulus 1.76 GPa
255 ksi
ISO 178
SABIC Innovative Plastics LNP STAT-KON SX90398 PA 12
LNP STAT-KON* SX90398 is a compound based on Nylon 12 resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
Flexural Modulus 1.76 GPa
255 ksi
ASTM D790
Star Plastics PC/PBTQX7008 Molding Grade PC/PBT
Information provided by Star Plastics, Inc.
Flexural Modulus 1.76 GPa
255 ksi
ASTM D790
Techmer ES Plastiblend® PA6/6,6 GF60 HS L 60% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, Copolymer and Lubricat..
Flexural Modulus 1.76 GPa
255 ksi
ASTM D790
Techmer ES Statiblend® PA12 CB
Availability: North AmericaForms: PelletsAdditive: Carbon BlackFeatures: ConductiveAppearance: BlackTPCI# 9872105Information provided by TP Composites, Inc.
Flexural Modulus 1.76 GPa
255 ksi
ASTM D 790
Styrolution PS 5310 HIPS
Excellent ESCRGood ToughnessMatte easily decorated finishInformation provided by Styrolution
Flexural Modulus 1.76 GPa
255 ksi
ASTM D 790
Styrolution PS 7120 HIPS
Excellent ESCR to foodstuffs and PUR foamsGood low temperature impact strengthHigh relative stiffness/potential to down gauge sheetUL Classification 94 HBInformation provided by Styrolution
Flexural Modulus 1.76 GPa
255 ksi
ASTM D 790
SABIC Innovative Plastics Noryl GTX GTX6010 PPE+PA6 (Asia Pacific)
PA6 based unfilled GTX. High impact.This data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Modulus 1.76 GPa
255 ksi
Tangent; ASTM D790
Washington Penn Homopolymer Polypropylene 10% Calcium Carbonate Filled
Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa..
Flexural Modulus 1.76 GPa
255 ksi
0.05 in/min, 1% secant; ASTM D-790A
Braskem FT200WV Homopolymer Polypropylene
Description: Good mold release, nucleated, excellent rigidity and hardness.Applications: Suggested uses include housewares, caps and closures, fast-cycle injection molding.Process: Injection Molding..